Abstract
This chapter is an account of the various events that led to the decline of the integrated steel industry during the 1950s. These include the steel strike of 1959, the improvements in technology and increase in imports since 1950s, widespread closures of steel companies, the decline of the minimill industry, and the rapid growth of Mittal Steel.
Topics
Steelmaking
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
The Decline of the Integrated Steel Industry, The History of Metals in America, By Charles R. Simcoe;Edited By Frances Richards, ASM International, 2018, p 207–218, https://doi.org/10.31399/asm.tb.hma.t59250207
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
The Integrated Steel Industry—1901 to 1959
The History of Metals in America
History and Primary Steel Processing
Steels: Processing, Structure, and Performance (Second Edition)
Overview of Iron and Steel Manufacturing
Iron and Steel Castings Engineering Guide
The Toolmakers
The History of Metals in America
Thermal Spray Applications in the Steel Industry
Thermal Spray Technology
Fractured Suspension Bar
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
The Steel Minimills
The History of Metals in America