Chapter 16: Surface Finishing
-
Published:2008
Abstract
This chapter discusses the functions of surface treatments important for stainless steel, namely the removal of oxide scale and cleaning, brightening, and coloring of the stainless surface. Details on the main methods of producing aesthetic surface finishes are also provided.
You do not currently have access to this chapter.
Citation
Surface Finishing, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 193–199, https://doi.org/10.31399/asm.tb.ssde.t52310193
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Cleaning, Pretreatment, and Maintenance of Surfaces
Aluminum Science and Technology
Design for Surface Finishing
Materials Selection and Design
Cleaning and Rust Protection
Practical Induction Heat Treating (Second Edition)
Surface Engineering of Copper and Copper Alloys
Surface Engineering
Coloring Anodized Aluminum
Aluminum Science and Technology
Forging of Stainless Steels
Metalworking: Bulk Forming
Thermal Aspects of Surface Finishing Processes
Surface Engineering
Cleaning and Finishing
Titanium: A Technical Guide (Second Edition)
Finishing and Coating
Metals Fabrication Understanding the Basics
The Life of Harry Brearley (1871–1948)
The History of Stainless Steel