Chapter 15: Machining
-
Published:2008
Abstract
This chapter focuses on the metallurgical factors governing the machinability of stainless steels. It begins by describing the chemistry, cleanliness, structure, processing history, and the cross-section size of the stock of the different grades of stainless steel. This is followed by a general description of the machining behavior of the stainless steel families, namely ferritic, martensitic, austenitic, precipitation hardening, duplex, and super stainless steels. The beneficial effect of controlled inclusions is then discussed. The chapter ends with a section providing information on high-speed tool steel and carbide tooling, along with tool coatings and coolants applicable to stainless steel.
Machining, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 181–191, https://doi.org/10.31399/asm.tb.ssde.t52310181
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.