Chapter 7: Duplex Stainless Steels
-
Published:2008
Abstract
This chapter provides information on the structure, design aspects, mechanical properties, forming, machining, and corrosion resistance characteristics of duplex stainless steels. The different types of corrosion covered are general corrosion, pitting corrosion, crevice corrosion, and stress corrosion cracking.
You do not currently have access to this chapter.
Citation
Duplex Stainless Steels, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 91–107, https://doi.org/10.31399/asm.tb.ssde.t52310091
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Corrosion Resistance of Stainless Steels and Nickel Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Chemical and Process Industry Applications
Stainless Steels for Design Engineers
Corrosion Types
Stainless Steels for Design Engineers
Nickel and Nickel Alloys
Alloying Understanding the Basics
Corrosion Resistance of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Coping with Corrosion
Metallurgy for the Non-Metallurgist (Second Edition)
Localized Corrosion
Fundamentals of Electrochemical Corrosion
Corrosion of Wrought Stainless Steels
Corrosion: Materials
Corrosion of Titanium and Titanium Alloys
Corrosion: Materials
Corrosion of Duplex Stainless Steel Weldments
Corrosion of Weldments