Chapter 10: Tempering of Martensite
-
Published:1999
Abstract
This chapter describes the effects that can be observed by light microscopy when a steel in the hardened condition, consisting of martensite and possibly some retained austenite, is heated at subcritical temperatures. It includes micrographs that illustrate the effect of carbide precipitation, the decomposition of retained austenite, and recovery and recrystallization. It also includes images that reveal the characteristic structures produced by tempering medium-carbon hypoeutectoid and hypereutectoid steels as well as the effects of plastic deformation, austenitic grain size, and temper brittleness.
Sign in
ASM members
Member Sign InTempering of Martensite, Light Microscopy of Carbon Steels, By Leonard E. Samuels, ASM International, 1999, p 283–307, https://doi.org/10.31399/asm.tb.lmcs.t66560283
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field