Appendix: Hardness Conversions
-
Published:2015
This appendix is a compilation of approximate equivalent hardness numbers and tensile strengths for carbon and alloy steels in the annealed, normalized, and quenched-and-tempered conditions.
You do not currently have access to this chapter.
Citation
Hardness Conversions, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 647–650, https://doi.org/10.31399/asm.tb.spsp2.t54410647
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Steel Cross Reference
Heat Treating of Irons and Steels
Introduction to Gear Heat Treatment
Heat Treatment of Gears A Practical Guide for Engineers
Hardenability Curves
Properties and Selection: Irons, Steels, and High-Performance Alloys
Carbonitriding Gears
Heat Treatment of Gears A Practical Guide for Engineers
Thermal Properties of Carbon and Low-Alloy Steels
Heat Treating of Irons and Steels
Carbon Steels and Alloy Steels Used in Warm and Hot Working
Induction Heating and Heat Treatment
Cracking on the Parting Line of Closed-Die Forgings
Handbook of Case Histories in Failure Analysis
Classifications and Designations of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Forging of Carbon and Alloy Steels
Metalworking: Bulk Forming
Compositions of Standard Alloy Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels