Abstract
This datasheet provides information on composition limits, fabrication characteristics, processing effects on physical and mechanical properties, and applications of aluminum alloy 7039.
You do not currently have access to this chapter.
Citation
7039: Armor Plate, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 418–419, https://doi.org/10.31399/asm.hb.v02b.a0006730
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
2519 Armor Plate and Cryogenic Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6061 and Alclad 6061 General Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys