7349: Extrusion Alloy
-
Published:2019
Abstract
The extrusion alloy 7349 was developed by Pechiney and introduced in 1994 to provide higher strength properties than incumbent 7x75 and 7150 alloys. This datasheet provides information on composition limits and processing effects on mechanical properties of this aluminum alloy. Performance comparisons of alloys 7349-T6511 with 7175-T76511 and 7349-T7651 with 7175-T77511 are also illustrated.
7349: Extrusion Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 454, https://doi.org/10.31399/asm.hb.v02b.a0006745