2195: Al-Li Plate Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy and processing effects on mechanical properties of Al-Li plate alloy 2195. A figure provides a performance comparison of 2195-T84 and 2219-T87 alloys.
You do not currently have access to this chapter.
Citation
2195: Al-Li Plate Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 316, https://doi.org/10.31399/asm.hb.v02b.a0006608
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
2196 and 2296 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Transistor Characterization: Physics and Instrumentation
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Overview of the Materials Selection Process
Materials Selection and Design
Surface Hardening
Steels: Processing, Structure, and Performance (Second Edition)
Properties of Liquid Lubricants
Friction, Lubrication, and Wear Technology
Principles of Alloying
Alloying Understanding the Basics
Vacuum Infusion
Composites
Out-of-Plane Analysis
Composites
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Modeling of Porosity Formation during Solidification
Metals Process Simulation