2011 and 2012: Free Machining Aluminum Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and general applications of free machining aluminum alloys 2011 and 2012. The effect of cutting speed on cutting force for different aluminum alloys is also illustrated.
You do not currently have access to this chapter.
Citation
2011 and 2012: Free Machining Aluminum Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 290–291, https://doi.org/10.31399/asm.hb.v02b.a0006595
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6061 and Alclad 6061 General Structural Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
5083 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys