Abstract
This article lists temper designations and their definitions for aluminum alloys along with their product forms used in the United States (ANSI H35.1), Europe (EN 515), and internationally (ISO 2107).
Topics
Aluminum alloys
You do not currently have access to this chapter.
Citation
Aluminum Alloy Temper Designations and Definitions, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 597–599, https://doi.org/10.31399/asm.hb.v02b.a0006622
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Aluminum Alloy Nomenclature and Temper Designations
Heat Treating of Nonferrous Alloys
Heat-Treatable Aluminum Alloy Temper Designations
Aluminum: Technology, Industry, and Applications
Aluminum Alloy Nomenclature and Temper Designations
Aluminum Science and Technology
Aluminum
Elements of Metallurgy and Engineering Alloys
Selection and Applications of Magnesium and Magnesium Alloys
Metals Handbook Desk Edition (2nd Edition)
Introduction to Copper and Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
6101 and 6201 Electrical Bus Conductor Alloy
Properties and Selection of Aluminum Alloys
Aluminum in Ground Transportation
Aluminum: Technology, Industry, and Applications