Abstract
This datasheet provides information on key alloy metallurgy and processing effects on tensile properties and fracture toughness of alloy 7065. Strength-toughness minima for aluminum plate alloy 7065 are presented.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
7065: High-Strength, Tough, Corrosion-Resistant Plate, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 430, https://doi.org/10.31399/asm.hb.v02b.a0006735
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
7255 High-Strength, Fatigue-Resistant Plate
Properties and Selection of Aluminum Alloys
7097 Plate Alloy
Properties and Selection of Aluminum Alloys
7449 Very High-Strength Plate and Extrusion Alloy
Properties and Selection of Aluminum Alloys
7475 Controlled-Toughness Sheet and Plate Alloy
Properties and Selection of Aluminum Alloys
Mechanical Properties Data for Selected Aluminum Alloys
Mechanics and Mechanisms of Fracture An Introduction
Mechanical Properties Data for Selected Steels
Mechanics and Mechanisms of Fracture An Introduction
Mechanical Properties of Beryllium
Beryllium Chemistry and Processing
Powder Metallurgy
Titanium: A Technical Guide (Second Edition)
Properties and Selection of Powder Metallurgy Titanium and Its Alloys
Powder Metallurgy
Melting, Casting, and Powder Metallurgy
Titanium Physical Metallurgy, Processing, and Applications