380.0, A380.0, and B380.0: General-Purpose Die-Casting Alloys
-
Published:2019
Abstract
The aluminum alloys 380.0, A380.0, and B380.0 are widely used for making general-purpose die castings. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, fabrication characteristics, and application characteristics of these 3xxx series alloys.
380.0, A380.0, and B380.0: General-Purpose Die-Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 565–566, https://doi.org/10.31399/asm.hb.v02b.a0006575