5050: General-Purpose Alloy
-
Published:2019
Abstract
The general-purpose alloy 5050 is a binary aluminum-magnesium alloy with more magnesium content than 5005. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series alloy.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
5050: General-Purpose Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 350–351, https://doi.org/10.31399/asm.hb.v02b.a0006694
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
5154 and 5154A Al-3.5Mg Alloy
Properties and Selection of Aluminum Alloys
535.0, A535.0, and B535.0 Al-Mg High-Strength Casting Alloy
Properties and Selection of Aluminum Alloys
511.0, 512.0 and 513.0 Al-Mg Moderate-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5083 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
6463 Bright-Finishing Extrusion Alloy
Properties and Selection of Aluminum Alloys