2297 and 2397: Plate for Fatigue Critical Applications
-
Published:2019
Abstract
Alloys 2297 and 2397 were developed for thick plate integral structures. This datasheet provides information on composition limits of these 2xxx series alloys and processing effects on mechanical properties of alloy 2297-T87 plate. A figure provides a performance comparison of 2297-T87 and 2124-T851 plates.
You do not currently have access to this chapter.
Citation
2297 and 2397: Plate for Fatigue Critical Applications, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 323, https://doi.org/10.31399/asm.hb.v02b.a0006612
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
7072 Cladding and Fin Stock
Properties and Selection of Aluminum Alloys
2040 High-Temperature Strength Alloy
Properties and Selection of Aluminum Alloys
7349 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7076 High-Strength Forging Alloy
Properties and Selection of Aluminum Alloys
Mechanical Properties and Testing of Titanium Alloys
Titanium Physical Metallurgy, Processing, and Applications
2524 Tough Moderate-Strength Sheet and Thin Plate
Properties and Selection of Aluminum Alloys
2196 and 2296 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Tribological Properties of Copper Alloys
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Stress-Corrosion Cracking of Magnesium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)