Abstract
Steel, heated in contact with air at temperatures in the tempering range, takes on various temper colors due to the formation of a thin oxide film. This article provides detailed information on temper colors for plain carbon steel, especially on the effects of time and temperature.
You do not currently have access to this chapter.
Citation
Temper Colors for Steels, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 550–551, https://doi.org/10.31399/asm.hb.v04d.a0005997
Download citation file:
Related Book Content
Acoustical Characterization
Steel Heat Treating Technologies
Heating and Holding Times
Steel Heat Treating Technologies
Iron and Steel
Elementary Materials Science
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)
Air-Hardening, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Heat Treatment Problems Associated with Design and Steel Selection
Heat Treating of Irons and Steels
High-Carbon, High-Chromium, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Cold and Cryogenic Treatment of Steel
Steel Heat Treating Fundamentals and Processes
Oil-Hardening Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Mold Steels
Tool Steels (Fifth Edition)