Ductile cast irons are heat treated to create matrix microstructures and associated mechanical properties not readily obtained in the as-cast condition. This article provides a detailed account of the general characteristics of ductile irons. It discusses the most important heat treatments of ductile irons, namely, stress relieving, austenitizing, annealing, normalizing, quenching, martempering, austempering, and surface hardening. The article elucidates the effects of these heat treatments on the mechanical properties of the ductile irons.
K. Hayrynen, Heat Treating and Properties of Ductile Iron, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 508–521, https://doi.org/10.31399/asm.hb.v04d.a0005937
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.