Failure analysis results were employed to identify a better alloy. Chipper knives used in the field to chip logs failed frequently. The knives were made of alloys with a composition of Fe-0.48C-0.30Mn-0.90Si-8.50Cr-1.35Mo-1.20W-0.30V. The development of tougher alloy steel with superior properties was initiated. The nominal composition of Fe-0.50C-0.30Mn-0.40Si-5.00Cr-2.00Mo was developed which achieved the goals of edge retention, resistance to softening under frictional heating, wear resistance, ease of heat treatment, dimensional stability in heat treatment, grindability, and low alloy cost. A chip harvester made from this composition was tested in field with older composition knives. It was found that the new knives outperformed the older knives. The key to the development was interpreted to be careful study of a number of failed knives with different problems used in different types of operations.
Failure of Chipper Knives, ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.conag.c0065827
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.