ASM Failure Analysis Case Histories: Processing Errors and Defects
Analysis of Contaminants on Grain-Boundary Fractures
-
Published:2019
Abstract
Cracks, with no other damage, were observed in a niobium alloy (Nb-106) part when it was pulled from several months of protective storage for assembly into a rocket nozzle. SEM views showed the cracks to be intergranular, with contaminant particles on a large number of the grain facets. EDX analysis showed they consisted of niobium and fluorine. Plastic replicas, prepared by standard TEM techniques, were analyzed with selected-area electron diffraction, showing a pattern match for niobium tetrafluoride. Auger analyses showed electron spectra containing peaks representing carbon, oxygen, nitrogen, fluorine, and chlorine. Investigation into the processing history of the part...
Sign in
ASM members
Member Sign InAnalysis of Contaminants on Grain-Boundary Fractures, ASM Failure Analysis Case Histories: Processing Errors and Defects, ASM International, 2019, https://doi.org/10.31399/asm.fach.process.c0045918
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!