Failure of Large Screen Spherical Bearing-Crushed Stone
By
H.W. Walton
H.W. Walton
The Torrington Company
Search for other works by this author on:
-
Published:2019
Abstract
The contamination of lubrication with powdered stone resulted in progressive wear of the internal surfaces of a bearing. Because of the motion of rollers, the inner race exhibited an unusual cyclic washboard wear pattern. Because of a lack of bearing conformity, wear progressed into severe coarse-grain spalling.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
H.W. Walton, Failure of Large Screen Spherical Bearing-Crushed Stone, ASM Failure Analysis Case Histories: Failure Modes and Mechanisms, ASM International, 2019, https://doi.org/10.31399/asm.fach.modes.c9001740
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Failure of Steel Rolling Mill Taper Bearing
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Glossary
Binder and Polymer Assisted Powder Processing
A Survey of the Causes of Failure of Rolling Bearings
ASM Failure Analysis Case Histories: Mechanical and Machine Components
Spalling of a Ball-Peen Hammer
Handbook of Case Histories in Failure Analysis
Contaminants
Systems Failure Analysis
Failure of a Crane Long-Travel Worm Drive Shaft
Handbook of Case Histories in Failure Analysis
Sledgehammer Chipping Failure
Handbook of Case Histories in Failure Analysis
Cracking at the Threads of Stud Bolts Used for Lifting Plastic Mold Dies
Handbook of Case Histories in Failure Analysis
High-Temperature Degradation of a Gas Turbine Transition Duct
ASM Failure Analysis Case Histories: Power Generating Equipment
Oxidation
Stainless Steels for Design Engineers