Pitting of 3003 Aluminum
By
R. Lee
R. Lee
Argonne National Laboratory
Search for other works by this author on:
-
Published:2019
Abstract
The Advanced Photon Source (APS) is a state-of-the-art synchrotron light source. The storage ring vacuum chamber is fabricated from 6061 extruded aluminum. Water connections to the vacuum chambers that were fabricated from 3003 aluminum had developed water leaks, which were subsequently remedied after considerable investigations.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
D.G. Ryding, D. Allen, R. Lee, Pitting of 3003 Aluminum, ASM Failure Analysis Case Histories: Failure Modes and Mechanisms, ASM International, 2019, https://doi.org/10.31399/asm.fach.modes.c9001691
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Inspection and Analysis of Aluminium Racks in Spent Fuel Storage Basins
ASM Failure Analysis Case Histories: Power Generating Equipment
Failure of a Helicopter Main Rotor Blade
Handbook of Case Histories in Failure Analysis
Ductile Overload Fracture of an Extension Ladder Made From 6061-T6 Aluminum Alloy Extrusions
ASM Failure Analysis Case Histories: Processing Errors and Defects
Fuel Line Corrosion
ASM Failure Analysis Case Histories: Air and Spacecraft
Wrought Aluminum Processes and Products
Aluminum Science and Technology
7049 and 7049A Extrusion and Forging Alloy
Properties and Selection of Aluminum Alloys
Collapse of Extension Ladders by Overloading of Side Rails
ASM Failure Analysis Case Histories: Household Products and Consumer Goods
Exfoliation Corrosion of HE.15 Aluminium Alloy
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Cavitation Erosion of a Water-Cooled Aluminum Alloy 6061-T6 Combustion Chamber
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
2324 High-Strength Plate
Properties and Selection of Aluminum Alloys