Investigating an Aircraft Disaster Available to Purchase
By
Ralph D. Barer
;
Ralph D. Barer
head, Materials Engineering Section, Defence Research Establishment Pacific
Search for other works by this author on:
Thomas S. Sterling
Thomas S. Sterling
Scientific Service Officer, Defence Research Establishment Valcartier
Search for other works by this author on:
-
Published:2019
Abstract
Applying general techniques of failure analysis, the authors deduced that an in-flight explosion brought down a passenger plane. Other evidence pinpointed the location of the explosive, an important factor in establishing responsibility.
You do not currently have access to this chapter.
Citation
Ralph D. Barer, Thomas S. Sterling, Investigating an Aircraft Disaster, ASM Failure Analysis Case Histories: Air and Spacecraft, ASM International, 2019, https://doi.org/10.31399/asm.fach.aero.c9001729
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Investigation of a Passenger Airline Crash
ASM Failure Analysis Case Histories: Air and Spacecraft
Aircraft Accident Caused by Explosive Sabotage
Handbook of Case Histories in Failure Analysis
Failure Analysis of a Large Blender in a Chemical Plant
ASM Failure Analysis Case Histories: Chemical Processing Equipment
Integrated Analysis of an Autoclave Failure
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
The Role of Metallography and Fractography in the Analysis of Gun Tube Failures
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Explosion of the Terra Ammonium Nitrate Plant, Port, Neal, Iowa
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Pressure Vessel from a High-Pressure Vibratory Autoclave Burst by Explosion
ASM Failure Analysis Case Histories: Chemical Processing Equipment
Assessment of Damage to Structures and Equipment Resulting from Explosion, Fire, and Heat Events
Analysis and Prevention of Component and Equipment Failures
Brittle Fracture Explosive Failure of a Pressurized Railroad Tank Car
Handbook of Case Histories in Failure Analysis
Failure of Stainless Steel Springs Used in an Oil Ring Lip Seal
Handbook of Case Histories in Failure Analysis