A failed 25 x 32 mm (1 x 1 in.) cadmium-plated 1040 carbon steel countersunk head type nose gear door securing bolt with a common screwdriver slot was examined. Fracture originated at a thread root and propagated across the cross section. The topography of the fracture was excessively rough and more granular than would be expected from pure mechanical fatigue. This indicated an allied corrosion mechanism. Cracks other than the one leading to failure were observed. Metallographic examination of the bolt cross section showed many cracks typical of stress-corrosion damage. It was concluded that the bolt failed by a...
Sign in
ASM members
Member Sign InFailure of Nose Gear Door Bolts, ASM Failure Analysis Case Histories: Air and Spacecraft, ASM International, 2019, https://doi.org/10.31399/asm.fach.aero.c0006432
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.