Stress Corrosion Cracking of Expansion Bellows of Steam Main
-
Published:2019
Abstract
Several articulated bellows of 10 in. ID developed leakage from the convolutions after a service life of some 18 months. One of the units received from examination showed cracking at the crown of a convolution and at the attachment weld to the pipe. Sectioning of the bellows revealed many others cracks on the internal surface which did not penetrate to the outside. Microscopical examination showed multiple intergranular, tree-like cracking typical of stress-corrosion cracking. Concentration of sodium hydroxide occurred in the bellows unit and the stress-corrosion cracking which developed was of the form known as caustic cracking. It was recommended...
Sign in
ASM members
Member Sign InStress Corrosion Cracking of Expansion Bellows of Steam Main, ASM Failure Analysis Case Histories: Power Generating Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.power.c9001398
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field