ASM Failure Analysis Case Histories: Automobiles and Trucks
Failure of an Automobile Transmission Stick-Shift
-
Published:2019
Abstract
A stick-shift from an automobile transmission failed in service. Failure occurred by stable fatigue crack propagation at locations R and L. Plausibly, the crack initiated at location R due to maximum tensile stress, which was perhaps further concentrated by a surface imperfection. As the crack progressed, the service load shifted to the section marked L. This overload on location L appears to have caused another fatigue crack that propagated first over the smooth-banded region. Catastrophic failure occurred when the component became unstable under the applied load.
Sign in
ASM members
Member Sign InFailure of an Automobile Transmission Stick-Shift, ASM Failure Analysis Case Histories: Automobiles and Trucks, ASM International, 2019, https://doi.org/10.31399/asm.fach.auto.c0048535
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.