ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Perforation of a Nickel-Base Alloy Kiln
-
Published:2019
Abstract
A kiln, 7.6 m (25 ft) long with a 1 m (3 ft) internal diameter and a 6.3 mm (0.25 in.) wall thickness, is used to regenerate spent charcoal returned by water utilities. This charcoal contains up to 0.57% S and 2.04% Cl. The kiln is made of Inconel 601 (N06601) welded using Inconel 617 (N06617) as a filler alloy. Wet charcoal is fed in at one end of the kiln and travels while being tumbled within the inclined rotating vessel. Temperatures range from 480 deg C (900 deg F) (Zone 1) to 900 deg C (1650 deg F)...
Sign in
ASM members
Member Sign InPerforation of a Nickel-Base Alloy Kiln, ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.steel.c0091757
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field