ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment documents more than 30 cases of structural and/or functional failure of components used in blast furnaces, melters, casters, rolling mills, heat-treating and brazing furnaces, and industrial ovens and kilns. The cases describe the investigation, identify the primary cause, and include remedial solutions. These case histories have been compiled from a wide variety of ASM International publication types, including ASM Handbook volumes, conference proceedings, technical books, journals, and magazines.
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
https://doi.org/10.31399/asm.fach.steel.9781627082327
ISBN (electronic): 978-1-62708-232-7
Publisher: ASM International
Published: 2019
Download citation file:
Table of Contents
-
Blast Furnace Equipment
-
Damaged Copper Hot Water PipeByEgon KauczorEgon KauczorStaatliches Materialprüfungsamt an der FachhochschuleSearch for other works by this author on:Published:01 June 2019
-
Fractured Recuperator Made of Heat Resistant Cast SteelByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Oxidized Recuperator PipesByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
-
Brazing Furnaces
-
Examination of an Oxidized Heating CoilByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
-
Heat Treating Equipment
-
Cracked Disks of Fan Made of Heat Resistant SteelByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Scaling of Resistance Heating Elements in a Through-Type Annealing FurnaceByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Industrial Ovens and Kilns
-
Integrated Analysis of an Autoclave FailureByW. J. D. ShawW. J. D. ShawDept. of Mechanical Engineering, University of CalgarySearch for other works by this author on:Published:01 June 2019
-
-
Metal Casting Equipment
-
Rolling Mill Equipment
-
Broken Back up Rolls from a Broad Strip MillByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Broken Rim of a Rolling Mill TransmissionByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Failure of Recuperator with Austenitically Welded PipesByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Failure of Steel Rolling Mill Taper BearingByH.W. WaltonH.W. WaltonThe Torrington CompanySearch for other works by this author on:Published:01 June 2019
-
Fractured Swivel HeadByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
Influence of Microstructure on the Premature Failure of a Second-Intermediate Sendzimir Mill Drive RollByA. Ray;A. RayPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:D. Mukherjee;D. MukherjeePhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:B. Sarkar;B. SarkarPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:S. MishraS. MishraPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:Published:01 June 2019
-
Microstructural Features of Prematurely Failed Hot-Strip Mill Work Rolls: Some Studies in Spalling PropensityByAmitava Ray;Amitava RayPhysical Metallurgy Group, Research and Development Centre for Iron and Steel, Steel Authority of India LimitedSearch for other works by this author on:M.S. Prasad;M.S. PrasadPhysical Metallurgy Group, Research and Development Centre for Iron and Steel, Steel Authority of India LimitedSearch for other works by this author on:S.K. Dhua;S.K. DhuaPhysical Metallurgy Group, Research and Development Centre for Iron and Steel, Steel Authority of India LimitedSearch for other works by this author on:S.K. Sen;S.K. SenPhysical Metallurgy Group, Research and Development Centre for Iron and Steel, Steel Authority of India LimitedSearch for other works by this author on:S. JhaS. JhaPhysical Metallurgy Group, Research and Development Centre for Iron and Steel, Steel Authority of India LimitedSearch for other works by this author on:Published:01 June 2019
-
Working Roll with Shell-Shaped FracturesByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
-
Steel and Metal Processing Equipment
-
Case of Metal Dusting on HK40 HyL III Radiant Pipe Heat ExchangerByPublished:01 June 2019
-
Failure of a Steel Pot Used for Melting Magnesium AlloysByLawrence J. KasharLawrence J. KasharDirector, Metallurgical Services Scanning Electron Analysis Laboratories, Inc.Search for other works by this author on:Published:01 June 2019
-
Low Cycle Thermal Fatigue and Fracture of Reinforced PipingByW.J. O'Donnell;W.J. O'DonnellO'Donnell & Associates, Inc.Search for other works by this author on:J.R. KenrickJ.R. KenrickEckert Seamans Cherin & MellottSearch for other works by this author on:Published:01 June 2019
-
Metallurgical Evaluation of a Five Inch Cylindrical Induction MelterByK.J. ImrichK.J. ImrichSavannah River Technology CenterSearch for other works by this author on:Published:01 June 2019
-
Metallurgical Investigation of a Prematurely Failed Roller Bearing Used in the Support and Tilting System of a Steel Making Converter Used in an Integrated Steel PlantByAmitava Ray;Amitava RayPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:S.K. Dhua;S.K. DhuaPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:K.B. Mishra;K.B. MishraPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:S. JhaS. JhaPhysical Metallurgy Group, Research & Development Centre for Iron & Steel, Steel Authority of India LimitedSearch for other works by this author on:Published:01 June 2019
-