Fractured Post of a Loading Gear Available to Purchase
-
Published:2019
Abstract
In a shipyard one of the two posts of a loading gear fractured under a comparatively small load at the point where it was welded into the ship’s deck. The post consisted of several pipe lengths that were produced by longitudinal seam welding of 27 mm thick sheets. The sheet metal was a construction steel of 60 to 75 kp/sq mm strength. Thick-walled parts of steels of such high strength must be preheated to approximately 200 deg C along the edges prior to welding to minimize the strong heat losses by the cold mass of the part. In the case under investigation this either was not done at all or the preheating was not high enough or sufficiently uniform. This damage was therefore caused by a welding defect.
Friedrich Karl Naumann, Ferdinand Spies, Fractured Post of a Loading Gear, ASM Failure Analysis Case Histories: Offshore, Shipbuilding, and Marine Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.marine.c9001210
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.