Sucker-rod pumps are operating in very aggressive environments in oil well production. The combined effect of a corrosive environment and significant mechanical loads contribute to frequent cases of failure of the rod string during operation. Standards and recommendations have been developed to control and avoid those failures. This study presents various failure cases of sucker rods in different applications. The heat treatment of the steel material and the resulting microstructure are an important factor in the behavior of the sucker rod. A spheroidized microstructure presents a weaker resistance to corrosion affecting the rod life. Non-metallic inclusions are a pitting...
Sign in
ASM members
Member Sign InSofiane Benhaddad, Glen Lee, Role of Microstructure in Sucker Rod String Failures in Oil Well Production, ASM Failure Analysis Case Histories: Oil and Gas Production Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.petrol.c9001592
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field