Skip Nav Destination
ASM Failure Analysis Case Histories
ASM Failure Analysis Case Histories: Medical and Biomedical DevicesAvailable to Purchase
ASM International
ISBN electronic:
978-1-62708-226-6
Publication date:
2019
ASM Failure Analysis Case Histories: Medical and Biomedical Devices documents around 20 cases of structural and/or functional failure of bone plates, orthopedic prostheses and fixation devices, medical instruments, and surgical wire, pins, and screws. The cases describe the investigation, identify the primary cause, and include remedial solutions. These case histories have been compiled from a wide variety of ASM International publication types, including ASM Handbook volumes, conference proceedings, technical books, journals, and magazines.
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
https://doi.org/10.31399/asm.fach.med.9781627082266
ISBN (electronic): 978-1-62708-226-6
Publisher: ASM International
Published: 2019
Download citation file:
Table of Contents
-
Bone Plates
-
Fatigue Failures of Austenitic Stainless Steel Orthopedic Fixation DevicesByM.E. Stevenson;M.E. StevensonMetals & Materials EngineersSearch for other works by this author on:M.E. Barkey;M.E. BarkeyDepartment of Aerospace Engineering and Mechanics, University of AlabamaSearch for other works by this author on:R.C. BradtR.C. BradtDepartment of Metallurgical and Materials Engineering, University of AlabamaSearch for other works by this author on:Published:01 June 2019
-
Microstructural Analysis of Failure of a Stainless Steel Bone Plate ImplantByL.M. BonaccorsiL.M. BonaccorsiUniversity of MessinaSearch for other works by this author on:Published:01 June 2019
-
Retrieval and Analysis of Surgical Implants in Brazil: The Need for Proper RegulationByC.R.F. Azevedo;C.R.F. AzevedoLaboratory for Failure Analysis, Instituto de Pesquisas Tecnológicas do Estado de São PauloSearch for other works by this author on:E. Hippert, Jr.E. Hippert, Jr.Laboratory for Failure Analysis, Instituto de Pesquisas Tecnológicas do Estado de São PauloSearch for other works by this author on:Published:01 June 2019
-
Medical Instruments
-
Fracture of a Bone DrillByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:Published:01 June 2019
-
-
Orthopedic Prostheses
-
Metallurgical Failure Analysis of a Broken Compression Hip Screw Surgical ImplantByCharlie R. Brooks;Charlie R. BrooksChemical, Metallurgical and Polymer Engineering Department, The University of TennesseeSearch for other works by this author on:Ashok ChoudhuryAshok ChoudhuryChemical, Metallurgical and Polymer Engineering Department, The University of TennesseeSearch for other works by this author on:Published:01 June 2019
-
Surgical Wire and Screws
-
Pitting of TiN-Coated Back Surgery WiresPublished:01 June 2019