Chemical Attack of Acrylonitrile-Butadiene-Styrene Grips
-
Published:2019
Abstract
A set of plastic grips from an electric consumer product failed while in service. The grips had been injection molded from a general-purpose grade of ABS resin. The parts had cracked while in use after apparent embrittlement of the material. Investigation (visual inspection, SEM imaging, and micro-FTIR in the ATR mode) showed that the spectrum representing the grip surface contained absorption bands associated with ABS as well as additional bands of significant intensity. A spectral subtraction removed the bands associated with the ABS resin resulting in a very good match with glyceride derivatives of fats and oils. This supported...
Sign in
ASM members
Member Sign InChemical Attack of Acrylonitrile-Butadiene-Styrene Grips, ASM Failure Analysis Case Histories: Household Products and Consumer Goods, ASM International, 2019, https://doi.org/10.31399/asm.fach.homegoods.c0090427
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!