Materials Characterization
Low-Energy Electron Diffraction
-
Published:1986
Abstract
Low-energy electron diffraction (LEED) is a technique for investigating the crystallography of surfaces and overlayers adsorbed on surfaces. This article describes the principles of diffraction from surfaces, and elucidates the method of sample preparation to achieve diffraction patterns. The article describes the limitations of surface sensitive electron diffraction and discusses the applications of LEED with examples.