A failure occurred in buried brass (92% Cu, 8% Zn) piping used to carry drinking water in wet clay soil after less than two years in service. Investigation (visual inspection, chemical analysis of both the pipe surface and water, and a comparison of the corrosion failure of power station condenser tubing cooled by seawater for two copper alloys, an aluminum brass alloyed with arsenic (UNS C68700, ASTM B111, or Cu-Zn-20Al DIN17660), and a cupronickel 70-30 alloy with iron added (C71500, ASTM B111, or Cu-Ni-30Fe DIN17665)) supported the conclusion that the failure was caused by microbial induced corrosion by sulfate-reducing bacteria. No recommendations were made.