ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment
Cracked Eccentric Camshaft
-
Published:2019
Abstract
During dismantling of an eccentric camshaft of 340 mm diam that had worked for a total of 450,000 load reversals, it was found that it had cracked on both sides of the eccentric cam. The shaft was made of chromium-molybdenum alloy steel 34 Cr-Mo4 (Material No. 1.7220) according to DIN 17200. Microstructural examination showed the shaft had ran hot, and there were no material defects. The shaft probably was overstressed by torsion forces. The presence of surface checks on both sides of the cam lobe that were filled with bearing metal proved that overstressing occurred through galling of the end faces of the bearing liners.
Friedrich Karl Naumann, Ferdinand Spies, Cracked Eccentric Camshaft, ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.machtools.c9001242
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.