Forming of Aluminum Alloys
Revising author
-
Published:2018
Abstract
Aluminum and its alloys are among the more formable materials of commonly fabricated metals. This article discusses the formability, bendability, and springback of aluminum and its alloys. It describes the forming limit diagrams that illustrate the biaxial combinations of strain that can occur without splitting. The article reviews various bending methods, such as draw, compression, ram and press, roll, and stretch or tension bending. It describes the process variations of incremental sheet forming (ISF), such as single-point incremental forming, two-point incremental forming, and kinematic incremental sheet forming. The article concludes with a discussion on spinning, warm forming, and superplastic forming.
Victoria Burt, Forming of Aluminum Alloys, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 336–356, https://doi.org/10.31399/asm.hb.v02a.a0006527
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.