Die Casting
-
Published:2018
Abstract
Nearly two-thirds of the aluminum castings made in North America are produced using high-pressure die casting techniques. This article compares and contrasts traditional high-pressure die casting with an improved version that uses a vacuum to pull air out of the die in order to reduce porosity in as-cast parts. It begins by describing a typical cycle for a traditional cold-chamber die casting machine, using detailed illustrations to show how gas can become trapped in the liquid metal. It then presents various remedies, ultimately focusing on vacuum die casting for the production of high-integrity parts. In addition to vacuum technology, the article discusses casting alloys, dies, and cells, and describes some of the benefits of structural die castings.
Martin Hartlieb, Kevin Anderson, Die Casting, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 175–192, https://doi.org/10.31399/asm.hb.v02a.a0006525
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!