Photography of Fractured Parts and Fracture Surfaces
-
Published:1987
Abstract
This article discusses the preparation of photomacrographs of fracture surfaces. It provides useful information on the equipment used, such as view cameras, 35-mm single-lens-reflex cameras, and stereomicroscopes. The article describes the role of lenses, focusing, camera magnification, and selection of lens aperture in a microscopic system. It illustrates the lighting techniques employed in photography and highlights the use of different films. The article concludes with a list of auxiliary equipment used in fracture surface photography.
Theodore M. Clarke, Photography of Fractured Parts and Fracture Surfaces, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 78–90, https://doi.org/10.31399/asm.hb.v12.a0001833
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.