Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of P/M aluminum alloys (aluminum-lithium alloys) and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fracture surface, and corrosion-fatigue crack initiation and propagation of these alloys.
You do not currently have access to this chapter.
Citation
P/M Aluminum Alloys: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 440, https://doi.org/10.31399/asm.hb.v12.a0000622
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Nonarbitrary Crack Size Concept for Fatigue Crack Initiation
Mechanics and Mechanisms of Fracture An Introduction
Fatigue Failure Mechanisms
Characterization and Failure Analysis of Plastics
Fatigue Testing and Behavior of Plastics
Mechanical Testing and Evaluation
ASTM/ASME Alloy Steels: Atlas of Fractographs
Fractography
Polymers: Atlas of Fractographs
Fractography
Low-Carbon Steels: Atlas of Fractographs
Fractography
High-Carbon Steels: Atlas of Fractographs
Fractography
Wrought Aluminum Alloys: Atlas of Fractographs
Fractography
Damage Tolerance of Metals
Mechanics and Mechanisms of Fracture An Introduction
Alloy Design for Fatigue and Fracture
Fatigue and Fracture