This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of ASTM/ASME alloy steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the solidification cracking, creep failure, brittle fracture, fracture by overpressurization, inclusion effect, fatigue crack propagation, ductile fatigue striation, secondary cracking, intergranular fracture, and elevated-temperature fracture of alloy steels used in pressure vessels, steam boiler superheater tubes, and box-girder bridges.
ASTM/ASME Alloy Steels: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 291–296, https://doi.org/10.31399/asm.hb.v12.a0000609