Cemented Carbides: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of one specific type of cemented carbide, tungsten carbide. It also assists in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the brittle fracture, transgranular fracture, intergranular fracture, and crack propagation of the tungsten carbide.