Cobalt Alloys: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of cobalt alloys (cast Vitallium and cast ASTM F75 alloys) and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fatigue fracture, microcrack, and stair-step fracture surface of these alloys.
You do not currently have access to this chapter.
Citation
Cobalt Alloys: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 398, https://doi.org/10.31399/asm.hb.v12.a0000618
Download citation file:
Related Book Content
Characteristic Observations on Type 316LR Stainless Steel Screws That Failed by Fatigue
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Fatigue Initiation on Type 316LR Straight Bone Plate
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Maraging Steels: Atlas of Fractographs
Fractography
Gray Irons: Atlas of Fractographs
Fractography
Fatigue Fracture of a Type 316L Stainless Steel Angled Plate
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Broken Stem of Femoral Head Component of Total Hip Prosthesis Made From Cast Cobalt-Base Alloy
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Failure of a Stainless Steel Hip Fracture Fixation Device
Handbook of Case Histories in Failure Analysis
Fatigue Fracture of Titanium Alloy Knee Prostheses
Handbook of Case Histories in Failure Analysis
Fracture of a Cast Stainless Steel Femoral Prosthesis
Handbook of Case Histories in Failure Analysis