Polymers: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of polymers, including polycarbonate, polyethylene, and polyimide, and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the quasi-brittle fatigue crack propagation, brittle and ductile fracture, crack-growth mechanisms, tearing, fibrillation, and fatigue striations of these surfaces.
You do not currently have access to this chapter.
Citation
Polymers: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 479–480, https://doi.org/10.31399/asm.hb.v12.a0000630
Download citation file:
Related Book Content
Wrought Aluminum Alloys: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Cast Aluminum Alloys: Atlas of Fractographs
Fractography
Copper Alloys: Atlas of Fractographs
Fractography
ASTM/ASME Alloy Steels: Atlas of Fractographs
Fractography
P/M Aluminum Alloys: Atlas of Fractographs
Fractography
Fatigue Failure Mechanisms
Characterization and Failure Analysis of Plastics
Fatigue Testing and Behavior of Plastics
Mechanical Testing and Evaluation
Low-Carbon Steels: Atlas of Fractographs
Fractography