Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of cast aluminum alloys and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the brittle fracture, microvoid coalescence, fatigue striations, and microstructure of these alloys. The components considered include fractured sand-cast carrier trays, broken extension-housing yokes, helicopter tail-rotor drive assemblies, fractured bell-crank fittings, chain-hoist hooks, and automotive connecting rods.
Cast Aluminum Alloys: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 405–413, https://doi.org/10.31399/asm.hb.v12.a0000620
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.