Resin-Matrix Composites: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of a type of resin-matrix composites, carbon-epoxy composites. The fractographs illustrate the fracture modes found in composite prepregs, composite panels, solid rocket motor nozzles, and tension, flexural, compressive, and shear loadings.
You do not currently have access to this chapter.
Citation
Resin-Matrix Composites: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 474–478, https://doi.org/10.31399/asm.hb.v12.a0000629
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Effects of Composition, Processing, and Structure on Properties of Composites
Materials Selection and Design
Concrete and Asphalt: Atlas of Fractographs
Fractography
Nickel Alloys: Atlas of Fractographs
Fractography
Ceramics: Atlas of Fractographs
Fractography
Cobalt Alloys: Atlas of Fractographs
Fractography
Metal-Matrix Composites: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Electronic Materials: Atlas of Fractographs
Fractography
Maraging Steels: Atlas of Fractographs
Fractography
Introduction to Environmental Performance of Nonmetallic Materials
Corrosion: Materials