Fractography
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of pure irons and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the grain-boundary cavitation; slip lines; intergranular fracture; cleavage fracture; notch-impact fracture; oxide inclusions and blowholes; ductile rupture; impact fracture and tensile-test fracture surfaces; fatigue striations; and crack initiation and propagation of pure irons.
Sign in
ASM members
Member Sign InPure Irons: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 219–224, https://doi.org/10.31399/asm.hb.v12.a0000601