Welding, Brazing, and Soldering
Solid-State Transformations in Weldments[1]
-
Published:1993
Abstract
Solid-state transformations occurring in a weld are highly nonequilibrium in nature and differ distinctly from those experienced during casting, thermomechanical processing, and heat treatment. This article focuses on welding metallurgy of fusion welding of steels and highlights the fundamental principles that form the basis of many of the developments in steels and consumables for welding. Examples in the article are largely drawn from the well-known and relatively well-studied case of ferritic steel weldments to illustrate the special physical metallurgical considerations brought about by the weld thermal cycles and by the welding environment. The article provides information on welds in other alloy systems such as stainless steels and aluminum-base, nickel-base, and titanium-base alloys.
P. Ravi Vishnu, Solid-State Transformations in Weldments, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 70–87, https://doi.org/10.31399/asm.hb.v06.a0001341
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!