Overview of Weld Discontinuities
-
Published:1993
Abstract
This article provides an overview of the types of weld discontinuities that are characteristic of specialized welding processes. These welding processes include electron-beam welding, plasma arc welding, electroslag welding, friction welding, resistance welding, and diffusion welding. The article also describes the common inspection methods used to detect these discontinuities.
Overview of Weld Discontinuities, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1073–1080, https://doi.org/10.31399/asm.hb.v06.a0001472