Abstract
Coextrusion welding (CEW) is a solid-state process that produces a weld by heating two or more workpieces to the welding temperature and forcing them through an extrusion die. This article describes cold and hot CEW for common metals such as low-carbon steel, aluminum, aluminum alloys, copper, and copper alloys. Additional applicable materials include nickel, nickel-base alloys, zirconium, titanium, tantalum, and niobium.
Topics
Weld corrosion,
Brazing,
Soldering,
Welding,
Brazeability,
Process modeling and simulation,
Joinability,
Solderability,
Weldability,
Low-carbon steel,
Extrusion dies,
Aluminum alloys,
Copper alloys,
Nickel alloys,
Extrusion welding,
Aluminum,
Zirconium,
Niobium,
Tantalum,
Copper,
Nickel,
Titanium
You do not currently have access to this chapter.
Citation
Coextrusion Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 311, https://doi.org/10.31399/asm.hb.v06.a0001379
Download citation file:
Related Book Content
Forge and Coextrusion Welding
Welding Fundamentals and Processes
Corrosion of Nonferrous Alloy Weldments
Corrosion of Weldments
Corrosion by Ammonia
Corrosion: Environments and Industries
Corrosion of Nonferrous Alloy Weldments
Corrosion in the Petrochemical Industry (Second Edition)
Introduction to Corrosion of Nonferrous Metals and Specialty Products
Corrosion: Materials
Corrosion Characteristics of Structural Materials
Corrosion: Understanding the Basics
Heat Treating of Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Linear Thermal Expansion of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Refractory Metals
Elements of Metallurgy and Engineering Alloys
Corrosion of Nonferrous Alloy Weldments
Corrosion: Fundamentals, Testing, and Protection