Selection of Wrought Ferritic Stainless Steels
-
Published:1993
Abstract
This article describes the classification of ferritic stainless steels. It reviews the metallurgical characteristics of various ferritic grades as well as the factors that influence their weldability. The article provides a discussion on various arc welding processes. These processes include gas-tungsten arc welding (GTAW), gas-metal arc welding (GMAW), flux-cored arc welding (FCAW), shielded metal arc welding (SMAW), and plasma arc welding (PAW). The selection criteria for welding consumables are discussed. The article also explains the welding procedures associated with the ferritic stainless steels. It concludes with information on weld properties.
K.F. Krysiak, J.F. Grubb, B. Pollard, R.D. Campbell, Selection of Wrought Ferritic Stainless Steels, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 443–455, https://doi.org/10.31399/asm.hb.v06.a0001409
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!