Selection and Weldability of Non-Heat-Treatable Aluminum Alloys
By
C.E. Cross
;
C.E. Cross
Martin Marietta Astronautics Group
Search for other works by this author on:
-
Published:1993
Abstract
Non-heat-treatable aluminum alloys constitute a group of alloys that rely solely upon cold work and solid solution strengthening for their strength properties. This article focuses on the weldability and weld properties of different classes on non-heat-treatable aluminum alloys.
You do not currently have access to this chapter.
Citation
C.E. Cross, M.L. Kohn, Selection and Weldability of Non-Heat-Treatable Aluminum Alloys, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 537–540, https://doi.org/10.31399/asm.hb.v06.a0001418
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Selection and Weldability of Aluminum-Lithium Alloys
Welding, Brazing, and Soldering
Selection and Weldability of Advanced Titanium-Base Alloys
Welding, Brazing, and Soldering
Selection and Weldability of Dispersion-Strengthened Aluminum Alloys
Welding, Brazing, and Soldering
Selection of Wrought Ferritic Stainless Steels
Welding, Brazing, and Soldering
Selection of Cast Stainless Steels
Welding, Brazing, and Soldering
Selection and Weldability of Heat-Treatable Aluminum Alloys
Welding, Brazing, and Soldering
Selection of Wrought Martensitic Stainless Steels
Welding, Brazing, and Soldering
The Materials Selection Process
Metallurgy for the Non-Metallurgist (Second Edition)
Selection of Wrought Duplex Stainless Steels
Welding, Brazing, and Soldering
Modeling of Diffusion Bonding
Metals Process Simulation